1.The thickness of the heating tube wall is too thin, the material selection is wrong or the quality is wrong, the use of seam pipes. The general thickness of the pipe wall is 0.8 units, and if it is too thin, it will be vulnerable to external force or damage under use.
2.If the magnesium oxide powder inside the electric heater element is damp, it is also have the possibility to be broken.
3.The power setting of the heating element is too high, the surface load is too large, and the internal temperature is too high, which is easy to cause the internal expansion , resulting in tube explosion.
4.There are many kinds of magnesium oxide powder, the best is the modified magnesium oxide powder with high temperature resistance. If inferior magnesium oxide powder is used, when the electric heater element is working, the internal expansion will also occur, resulting in a tube explosion.
5.The outer tube material of the heating element may be thin thickness tube, or it may be a seam tube, which leads to easy crack.
6.The water used for heating may be groundwater, or tap water, with more impurities, easy to scale, too much scale is too thick, which will lead to the internal temperature of the heater element can not be diffused, resulting in explosion.